Brief: seam failures on 4 kg treat pouches were causing roughly 3% loss per container in summer shipping.
What we did: increased sealant gauge, widened the seal bar profile, and ran drop and compression tests at 35 °C before releasing production.
Result: failure rate below 0.2%, and a resealable zipper that survives repeated opening without tearing the laminate.